LT (LiTaO3) Lithium Tantalate Crystals – Electro-optic Crystal – Customized Products

Product ID: 6807


$100

LT (LiTaO3) Lithium Tantalate Crystals – Electro-optic Crystal – Customized Products

LiTaO3 crystals, also known as lithium tantalate crystals, or LT crystals for short, are electro-optical crystals with excellent overall performance. LiTaO3 crystals have the advantages of high optical damage threshold, low birefringence, transmission bandwidth, high optical transmittance, high sensitivity, wide transparency range, large electro-optical coefficient, no easy deliquescence, and stable chemical and physical properties, and are used in optical storage, transient recording, high-speed holographic cameras, and other related fields. It has a wide
range of applications in related fields such as optical storage, transient recording, high-speed holographic cameras, etc. With the increasing Li/Ta in LT crystals, its physical properties are also improved to different degrees, which is conducive to improving the performance of various functional devices and making them used in many important fields such as laser TV, laser ranging, radar, infrared military countermeasures, medical treatment, and atmospheric environment monitoring, and it is likely to open up new application fields.

Note:
$100 is a deposit, not the final price of the product. Please contact us for price if needed.

FEATURES
High sensitivity
Wide range of transparency
Large electro-optical coefficient
Not susceptible to deliquescence
High optical damage threshold
Stable chemical and physical properties

SPECTRA
Optical Storage
Transient recording
High-speed holographic camera

Crystal Properties

Crystal Structure Triangle, Space Group R3c, Point Group 3m
Crystal Cell Parameters a=5.154Å,c=13.781Å
Melting Point 1650℃
Curie Temperature 607℃
Mohs Hardness ~5.5
Density 7.46g/cm3
Dielectric Constant ea=54 ec=43(@100KH)
Transmission Range 400-4500nm
Electro-optic Coefficient r33=30.4pm/V
Refractive Index at 632.8nm no=2.176,ne=2.180
Nonlinear Optical Coefficient(P/m/V @1064nm) d22=2.0
d31=-1
d33=-21
Pyroelectric Coefficient ~2.3 ×10-4C/℃/m2
Optical Uniformity ~10-5
Absorption loss <0.15%/cm

 

Spectrum

TaorLab laser crystals